A comparative surface analysis of zirconia, titanium and titanium-zirconium dental implants

Research output: Contribution to journalArticlepeer-review

Abstract

Clinical Oral Implants Research. 26():46, SEP 2015 DOI: 10.1111/clr.45_12679 , Issn Print: 0905-7161 Publication Date: 2015/09/01
Original languageEnglish
JournalClinical Oral Implants Research
Publication statusPublished - 1 Sep 2015

Fingerprint

Dive into the research topics of 'A comparative surface analysis of zirconia, titanium and titanium-zirconium dental implants'. Together they form a unique fingerprint.